Home > What's New > How to make sintered NdFeB magnet additives?
How to make sintered NdFeB magnet additives? 2012-08-03
Ningbo Xinfeng Magnet sintered ndfeb magnet experience Nd-Fe-B alloy ingots or
scales broken by hydrogen, add a proprietary additive in the HD powder evenly
mixed together jet mill (JM). Addition amount about 0.03% -0.05% powder, this
additive is a multiple of organic compounds. Gene pro-oil, or C17H35-based.
Small amount of polarity genes, such as lipid-based, etc., it has the
appropriate length. JM magnetic powder particles in the course of repeated
impact and contact with the additive, it will face in each particle coating
layer thickness of about 5-8nm additive films, which play the following role. To
prevent the powder particles in contact with air, from the oxidation effect;
reduced static magnetic powder particles effects, reduce the reunion between the
powder particles played the role of dispersant; increase the mobility of the
powder particles with mobility, from the lubricant effect; favorable powder
particles in a magnetic field tended to enhance the orientation degree; the Br
can increase 0.02-0.04T, the energy product can also be increased accordingly.
It is worth noting that additives play a temperature of about 350 degrees, when
sintering temperature in the 400-420 degree heat for some time, so that
additives emitted from the magnets so as to avoid increasing carbon; additive of
some slight odor, in that material and pressure-type should be appropriate
protection; additive, forming pressure should be increased appropriately. JM
equipment additives on grinding chamber wall pipe and a slight corrosion.